PPS Product Flow Marks

ظاهرة المشكلة
Surface flow marks and ripples.
تحليل الأسباب
Low front temperature or unsteady filling.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
الحل
①Increase temperature; ②optimize the speed curve; ③enlarge the gate; ④fill smoothly.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
الخلاصة الأساسية
Flow marks are improved by temperature and speed.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future