Extrusion & Post
13 مشاهدة
PP Extrusion Temperature Setting
ظاهرة المشكلة
[Problem Phenomenon] Improper temperature for PP extrusion of film, sheet, and pipe; unstable quality
تحليل الأسباب
PP extrusion melt temperature 200-260°C adjusted by product; die temperature affects the surface; screen pack pressure differential monitoring; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based on experience alone
الحل
Extrusion melt temperature 200-260°C; die temperature matching; screen pack pressure differential monitoring; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
الخلاصة الأساسية
PP extrusion 200-260°C; die temperature determines the surface; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar future problems
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!