Injection Molding 6 مشاهدة

GPPS Transparent Part Flow Marks

ظاهرة المشكلة
Wavy flow marks appear on the product surface, especially obvious on transparent parts.
تحليل الأسباب
The melt front cools quickly, and subsequent melt pushes to form ripples; low material temperature and mold temperature and slow injection speed aggravate front cooling.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
الحل
①Appropriately increase melt temperature; ②increase mold temperature; ③increase injection speed; ④enlarge gates and runners.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
Flow marks reflect front temperature management problems; PS has good fluidity, and increasing temperature and speed can improve it.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence