Processing Machinery
5 مشاهدة
Improper Screw Configuration for PSU
ظاهرة المشكلة
In PSU processing, poor plasticization coexists with overheating degradation; screw load is heavy; equipment alarms are frequent; the process window cannot be stabilized.
تحليل الأسباب
PSU requires a single-flighted full-thread constant-pitch low-compression-ratio screw with an L/D ratio between 14~20; high-viscosity melt requires low-gear stepless speed regulation of 15~45 r/min; improper configuration causes loss of control over both plasticization and shear.
الحل
①Select a single-flighted full-thread constant-pitch low-compression-ratio screw; ②L/D ratio of 14~20; ③Speed of 15~45 r/min with low-gear stepless regulation; ④Precision wear-resistant screw and barrel set configuration.
الخلاصة الأساسية
PSU screw configuration has clear industry specifications; low speed protects the high-viscosity melt; precision wear-resistant configuration is the foundation of long-term stability.; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا