Injection Molding 8 مشاهدة

PVC Injection Flash

ظاهرة المشكلة
Parting line flash, needs trimming after demolding.
تحليل الأسباب
Insufficient clamping, excessive pressure; PVC viscosity drops sharply after decomposition making flash easier; parting line wear also induces it; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based solely on experience.
الحل
①Reduce injection/extrusion pressure; ②Calculate and increase clamping force; ③Check whether thermal degradation occurred (yellowing, black specks, odor); ④Repair parting line and moving part fitting clearance, match mold if necessary; ⑤Check parting line and moving part fitting clearance.
الخلاصة الأساسية
PVC flash 'also beware of degradation-induced viscosity drop': degradation makes PVC suddenly thin and flash; besides reducing pressure and increasing clamping, check back whether thermal degradation caused abnormal viscosity.
PVC; '2079851475616104452; flash; clamping; degradation