PVC Regrind Use Problems

ظاهرة المشكلة
After adding regrind, products yellow quickly, black specks increase, performance declines.
تحليل الأسباب
PVC regrind has consumed part of stabilizer and experienced heat history; crushed material contains moisture and dust; regrind's thermal stability reserve is discounted, easier to degrade; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based solely on experience.
الحل
①Regrind proportion controlled with additional stabilizer; ②Regrind dried and decontaminated; ③Downgrade use to non-appearance parts; ④Avoid multiple reuses; ⑤Establish correspondence ledger of regrind batches and performance.
الخلاصة الأساسية
PVC regrind = 'stabilizer reserve discounted': use less and cautiously, and add stabilizer; PVC regrind's heat history directly determines remaining stability, multiple reuse risk is extremely high.
PVC; regrind; yellowing; stabilizer; heat history