Processing Machinery 5 مشاهدة

PVC Nozzle Temperature

ظاهرة المشكلة
PVC nozzle repeatedly shows degradation yellow spots
تحليل الأسباب
Nozzle temperature locally too high or structural dead corner retention, PVC degrades first at nozzle; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based solely on experience.
الحل
Nozzle temperature take lower limit and heat uniformly; choose large-bore straight-through nozzle; regular cleaning; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
الخلاصة الأساسية
PVC nozzle should be straight-through large bore plus temperature lower limit; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
PVC nozzle yellow spot straight-through