PVC Blister Packaging
ظاهرة المشكلة
PVC blister shells had poor transparency and gel particles
تحليل الأسباب
Sheet plasticization quality and regrind ratio affect transparency; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
الحل
Select transparent-grade sheet; control regrind ratio; uniform '2079851475616104458 temperature; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
الخلاصة الأساسية
Blister transparency relies on sheet quality and temperature control; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!