Processing Machinery 5 مشاهدة

PVDF Product Welding

ظاهرة المشكلة
Welding joint problems.
تحليل الأسباب
PVDF can be hot-melt welded for pipe connections; welding temperature and time must be controlled.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
الحل
①Develop welding parameters; ②control welding temperature; ③perform strength and sealing verification; ④train operators.; After adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
PVDF welding is key to pipe installation; parameters and operation are equally emphasized.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; Include this case in the defect archive as a reference for troubleshooting similar problems in the future
PVDF;welding;hot-melt;pipe;sealing;parameters