Injection Molding
7 مشاهدة
PVDF Injection Mold Material and Corrosion
ظاهرة المشكلة
【Problem phenomenon】The runner and cavity surfaces of PVDF molding molds gradually corrode and roughen, and product appearance deteriorates accordingly
تحليل الأسباب
Trace HF acting over the long term corrodes ordinary mold steel, and corrosion products in turn contaminate the melt forming a vicious cycle; fluoroplastic molds require corrosion-resistant steel and surface treatment; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
الحل
Select corrosion-resistant stainless steel or hard chrome/nickel plating treatment for mold runners and cavities; regularly check runner surface condition; thoroughly clean when changing material to prevent cross corrosion; After adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
PVDF molds require corrosion-resistant material selection plus regular inspection; corrosion self-amplifies; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; Include this case in the defect archive as a reference for troubleshooting similar problems in the future
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا