Extrusion & Post 13 مشاهدة

TPE Overmolding Long-Term Delamination

ظاهرة المشكلة
Room temperature test passes, but delamination occurs after the customer uses it for a period of time.
تحليل الأسباب
Insufficient verification lacking environmental reliability testing; temperature cycling, chemical contact, long-term stress or ultraviolet slowly weaken interface strength.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
الحل
①Review the product use environment; ②supplement aging test, chemical resistance test or creep test; ③evaluate the long-term durability of adhesion; ④improve the verification plan.
الخلاصة الأساسية
Overmolding adhesion verification must cover the actual use environment; room temperature immediate testing is insufficient to guarantee long-term reliability.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
TPE;overmolding;delamination;reliability;aging test;verification