Material Drying 6 مشاهدة

TPE Regrind Drying

ظاهرة المشكلة
TPE products with regrind show bubbles and performance decline
تحليل الأسباب
Regrind absorbs moisture and accumulates heat history; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
الحل
Dry regrind separately; blending ratio not exceeding 20%; prohibited for performance parts; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
الخلاصة الأساسية
TPE regrind is dried and used in limited amounts; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
TPE regrind drying blending