Injection Molding
7 مشاهدة
TPU Injection Speed Control
ظاهرة المشكلة
After high-speed injection, burning occurs near the gate, while low speed produces flow marks and weld lines
تحليل الأسباب
TPU is shear-sensitive; shear heat from high-speed injection degrades the gate area; at low speed, the flow front cools and forms flow marks; medium-slow speed is the conventional strategy for TPU; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
الحل
①Injection speed controlled at medium-slow; ②Pass through the gate area at low speed; ③When flow marks occur, increase melt temperature to compensate; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
الخلاصة الأساسية
TPU speed strategy is stability-first; the balance between shear degradation and flow marks relies on medium-low speed plus temperature compensation; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!