EEA extrusion profile bending deformation
ظاهرة المشكلة
EEA extruded profiles show continuous bending after cooling, deflection >5mm/m
تحليل الأسباب
Uneven cooling of each face of the profile causing shrinkage difference; uneven die outlet flow velocity making each wall thickness of the profile different; haul-off and extrusion centerlines not aligned producing lateral force
الحل
1) Optimize the cooling system to ensure uniform cooling of each face; 2) Adjust the die to make the flow velocity of each wall uniform and wall thickness consistent; 3) Align the haul-off and extrusion centerlines; 4) Increase the sizing sleeve length, cool after full setting
الخلاصة الأساسية
Profile bending is caused by uneven cooling and uneven flow velocity; homogenization and alignment are the key to resolution