Injection Molding 5 مشاهدة

EMA '2079851475616104452 Cold Slug Marks

ظاهرة المشكلة
Cold slug marks appear near the gate of EMA injection molded products
تحليل الأسباب
Nozzle temperature low, causing residual material from the previous injection to cool and solidify in the nozzle; cold slug well design insufficient, cannot accommodate cold material; injection pressure insufficient
الحل
1) Increase nozzle temperature to 160-210°C; 2) Design a sufficiently large cold slug well in the mold; 3) Ensure fresh melt at the front of the nozzle before each injection; 4) Increase injection pressure to push cold material through the gate
الخلاصة الأساسية
Cold slug marks are caused by solidified residual material in the nozzle; increasing nozzle temperature and cold slug well design are key