Extrusion & Post 12 مشاهدة

Bending Deformation of PU Extruded Profiles

ظاهرة المشكلة
PU extruded profiles continuously bend after cooling, bending deviation >5mm/m
تحليل الأسباب
Cooling of profile faces uneven causing shrinkage differences; die exit flow velocity uneven making profile wall thicknesses different; haul-off and extrusion centerline misaligned producing lateral force
الحل
1) Optimize the cooling system to ensure uniform cooling of all faces; 2) Adjust the die to make flow velocity of each wall uniform and wall thickness consistent; 3) Align haul-off and extrusion centerline; 4) Increase sizing sleeve length, fully size then cool
الخلاصة الأساسية
Profile bending is caused by uneven cooling and uneven flow velocity; homogenization and alignment are the solution keys
PU extrusionbending deformationuniform coolinguniform flow velocitysizing sleeve

هل كان هذا مفيدًا؟

0 شخص وجدوا هذا مفيدًا