Injection Molding 7 مشاهدة

Product difficult to eject from the mold

ظاهرة المشكلة
The product is difficult to eject from the mold, requires increased demolding force, the product surface may be scratched or deformed
تحليل الأسباب
Mold cavity surface rough or damaged Injection pressure too high, product fits the cavity too tightly Cooling time insufficient, product not yet fully shrunk Improper release agent use or excessive amount Insufficient mold draft angle
الحل
Polish the mold cavity surface Appropriately reduce injection pressure Extend cooling time until the product is fully solidified Use release agent reasonably, avoid excess Increase the draft angle to 1-2°
الخلاصة الأساسية
Difficult demolding requires improving the mold surface and demolding conditions
difficult demoldingmold stickingdraft anglecooling