DSTDP vacuum vent section material overflow
ظاهرة المشكلة
DSTDP extrusion vacuum vent section material overflow, vent hole clogged
تحليل الأسباب
DSTDP melt viscosity low, overflowing at the vacuum vent section; vacuum vent section temperature on the high side, viscosity even lower, aggravating overflow; vent hole design improper
الحل
1) Lower vacuum vent section temperature 5-10°C to increase viscosity; 2) add baffle above the vent hole to prevent overflow; 3) increase screw speed to accelerate conveying and reduce residence
الخلاصة الأساسية
Material overflow is caused by low melt viscosity; temperature reduction and baffle are key