Extrusion & Post
12 مشاهدة
Glass Fibre extrusion pelletizing connected pellets
ظاهرة المشكلة
During Glass Fibre extrusion pelletizing, pellets connected between each other, not completely cut, forming bead-string shape
تحليل الأسباب
Glass Fibre soft, during pelletizing the knife cuts in but elastic recovery makes cut surfaces re-bond; pelletizing water temperature too low <40°C, not fully solidified; cutter speed not matched with extrusion speed
الحل
1) Raise pelletizing water temperature to 50-60°C, cut after full solidification; 2) increase cutter speed to ensure fast cutting; 3) cutter gap 0.01-0.02mm ensures clean cutting; 4) rotary cutter instead of flat cutting to reduce connected pellets
الخلاصة الأساسية
Connected pellets are caused by elastic recovery and low-temperature pelletizing; high-temperature water cutting and fast cutting are key
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا