Extrusion & Post 12 مشاهدة

Glass Fibre film excessive heat shrinkage

ظاهرة المشكلة
Glass Fibre film at 80°C heat shrinkage >12%, exceeding 5% dimensional stability requirement
تحليل الأسباب
Glass Fibre extrusion orientation releases upon heating causing large shrinkage; Glass Fibre thermal expansion coefficient large; film cooling froze a large amount of orientation stress
الحل
1) Reduce extrusion draw ratio to reduce orientation freezing; 2) film annealing treatment 60-80°C to release orientation stress; 3) add 5-10wt% rigid resin to reduce heat shrinkage; 4) biaxial stretching process to balance orientation
الخلاصة الأساسية
Film heat shrinkage is caused by orientation freezing; reducing draw ratio and annealing treatment are key
Glass Fibre filmheat shrinkageorientation releaseannealing treatmentbiaxial stretching