Glass Fibre poor chemical resistance
ظاهرة المشكلة
Glass Fibre product after soaking in acid-alkali solvent mechanical properties drop >30%
تحليل الأسباب
Glass Fibre has high affinity to specific chemicals, eroded and swelled; Glass Fibre molecular chains attacked by chemicals and broken
الحل
1) Select chemical-resistant grade; 2) slight crosslinking to reduce swelling; 3) product surface coating protection; 4) add chemical stabilizer
الخلاصة الأساسية
Poor chemical resistance is caused by Glass Fibre chemical affinity; selecting chemical-resistant grade and coating are key