Extrusion & Post
12 مشاهدة
MP vacuum section material overflow
ظاهرة المشكلة
MP extrusion vacuum section material overflow, vent hole blocked
تحليل الأسباب
MP melt viscosity low, overflowing at the vacuum section; vacuum section temperature high, viscosity lower, aggravating overflow; vent hole design improper
الحل
1) lower vacuum section temperature 5-10°C to increase viscosity; 2) add a baffle above the vent hole to prevent overflow; 3) increase screw speed to accelerate conveyance and reduce residence
الخلاصة الأساسية
material overflow is caused by low melt viscosity; lowering temperature and adding a baffle are key