MP insufficient mixing
ظاهرة المشكلة
after MP compounded with filler/additives, dispersion uneven, local agglomeration
تحليل الأسباب
screw mixing section length insufficient; kneading block number insufficient; improper feeding method, additives not fully contacting MP
الحل
1) increase screw mixing section length to 3-4D; 2) increase kneading block number; 3) feed additives through the side feed port later to increase mixing time
الخلاصة الأساسية
insufficient mixing is caused by improper screw design; increasing the mixing section is key