Material Drying
4 مشاهدة
Control of demolding abnormality in PEOX coating laundry pods
ظاهرة المشكلة
During PEOX coating production of laundry pods, the problem of large fluctuation in demolding occurs.
تحليل الأسباب
Mainly due to the processing temperature deviating from the window +60-100°C, moisture content >0.5% exceeding the standard, and insufficient cooling.
الحل
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
الخلاصة الأساسية
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا