Material Drying
6 مشاهدة
Control of demolding abnormality in PEOX '2079851475616104458 pharmaceutical films
ظاهرة المشكلة
During PEOX '2079851475616104458 production of pharmaceutical films, the problem of uneven demolding occurs.
تحليل الأسباب
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.3% exceeding the standard, and excessively long residence time.
الحل
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and shorten the residence time.
الخلاصة الأساسية
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.
هل كان هذا مفيدًا؟