Control of appearance abnormality in PEOX extrusion packaging
ظاهرة المشكلة
During PEOX extrusion production of packaging, the problem of not up to standard appearance occurs.
تحليل الأسباب
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.1% exceeding the standard, and insufficient cooling.
الحل
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
الخلاصة الأساسية
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.