Control of dissolution rate abnormality in PEOX calendering agricultural products
ظاهرة المشكلة
During PEOX calendering production of agricultural products, the problem of unstable dissolution rate occurs.
تحليل الأسباب
Mainly due to the processing temperature deviating from the window +70-90°C, moisture content >0.3% exceeding the standard, and insufficient cooling.
الحل
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and strengthen cooling.
الخلاصة الأساسية
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.