Extrusion & Post
12 مشاهدة
Regulation of die buildup of PPA in wire drawing Processing
ظاهرة المشكلة
The die buildup abnormality of the PPA processing aid in wire drawing production affects quality.
تحليل الأسباب
The die buildup of the PPA fluoropolymer is unsatisfactory at an addition amount of 0.02%, and the fluorine content needs to be optimized.
الحل
Adjust the PPA addition position combined with formulation adjustment.
الخلاصة الأساسية
The key to the performance of PPA lies in matching with the base resin.