Material Analysis
6 مشاهدة
Analysis and Resolution of transparency of Smooth MB in heat shrink film bags
ظاهرة المشكلة
When Smooth MB produces bags with heat shrink film, abnormal performance related to transparency occurs.
تحليل الأسباب
The main cause is improper parameter settings in the aspect of transparency, leading to processing instability.
الحل
Comprehensively resolve the transparency problem from the perspective of formulation optimization.
الخلاصة الأساسية
The control of transparency of Smooth MB is the key link in ensuring processing quality.
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا