Extrusion & Post 16 مشاهدة

POE extrusion dimensional instability

ظاهرة المشكلة
POE extruded product cross-section dimension fluctuates ±10%, with periodic changes in the length direction as well
تحليل الأسباب
Feeding amount unstable, feeding screw speed fluctuates; extrusion temperature periodically fluctuates ±5°C; haul-off speed does not match extrusion speed
الحل
1) Use loss-in-weight feeder to ensure stable feeding; 2) PID control of each extruder zone temperature with accuracy ±1°C; 3) Closed-loop control of haul-off speed linked with extrusion speed; 4) Control processing temperature at 160-200±5°C
الخلاصة الأساسية
Extrusion dimensional stability depends on feeding accuracy, temperature control and haul-off synchronization
POE extrusiondimensional stabilityfeeding controltemperature PIDhaul-off synchronization