Extrusion & Post 7 مشاهدة

thickness deviation Occurring in the die discharge Stage of Cast polypropylene film

ظاهرة المشكلة
thickness deviation occurs in the film during the die discharge stage, affecting production stability and product quality. Cast polypropylene film is sensitive to the process parameters of this stage.
تحليل الأسباب
(1) The process parameters of the die discharge stage are set improperly (2) The equipment condition or precision is insufficient (3) Raw material characteristics (cast extrusion, chill roll control, high transparency, good heat sealability) cause processing difficulties (4) The environmental conditions (temperature and humidity) are unsuitable (5) Improper operation or inadequate monitoring
الحل
(1) Optimize the process parameters of the die discharge stage, and control the temperature within the range of 230-270°C (2) Check and maintain the equipment to ensure operating precision (3) Select processing process parameters suitable for cast polypropylene film (4) Control the temperature and humidity of the production environment (5) Strengthen operation training and process monitoring
الخلاصة الأساسية
The process parameters of each stage of film production need to be precisely controlled; equipment condition and raw material quality are the foundation.
die dischargethickness deviationcast polypropylene filmprocess parametersequipment maintenance