Insufficient heat seal strength of linear low density polyethylene film (Variant: strengthened measures)

ظاهرة المشكلة
After film heat sealing, seal strength is low, and the seal cracks under stress. Insufficient heat seal strength affects packaging tightness, causing leakage in food packaging film. In particular, additional attention is needed on the original basis; this problem is more prominent and requires key attention.
تحليل الأسباب
(1) Heat seal temperature too low, insufficient melting (2) Insufficient heat seal pressure or time (3) Uneven film thickness, heat seal area too thin (4) Film surface contamination or additive exudation (5) Improper heat seal material selection (6) On the original basis, additional attention is needed as process parameter fluctuations or equipment status changes have aggravated this problem
الحل
(1) Adjust heat seal temperature according to the melting point of linear low density polyethylene, generally 10-20°C above the melting point (2) Increase heat seal pressure to 0.2-0.4MPa, heat seal time 0.5-2s (3) Ensure uniform film thickness, especially at heat seal areas (4) Control additive dosage, avoid surface exudation affecting heat seal (5) Use heat seal layer materials when necessary (such as LDPE, EVA, etc.) (6) And strengthen process monitoring; on the original basis, additional attention is needed, with special attention to parameter stability
الخلاصة الأساسية
Insufficient heat seal strength is caused by improper temperature, pressure, or time settings; heat seal process parameters need to be optimized. Targeted preventive measures need to be taken in different production scenarios.
heat seal strengthheat seal temperatureheat seal pressurefilm thicknessheat seal material