Processing Machinery 6 مشاهدة

Unreasonable die head flow channel design of heat-resistant polyethylene extruder (Variant: strengthened measures)

ظاهرة المشكلة
The flow velocity of the extrudate is uneven at various parts, and the cross-sectional dimensional deviation of the product is large. Die head flow channel design directly affects the uniformity and quality of the extrudate. Especially on the original basis, additional attention is needed, and this problem is more prominent and requires key attention.
تحليل الأسباب
(1) Unreasonable die head flow channel distribution, unequal flow path lengths at various parts (2) Die sizing section length insufficient (3) Dead corners in flow channel, material stagnates and degrades (4) Flow channel surface finish insufficient (5) Die head heating uneven (6) On the original basis, additional attention is needed: process parameter fluctuations or equipment state changes aggravate this problem
الحل
(1) Optimize flow channel design, use coat-hanger or manifold distributors to ensure equal flow path lengths (2) Increase die sizing section length to stabilize melt flow (3) Eliminate flow channel dead corners, all corners transition with arcs (4) Polish flow channel surface to Ra≤0.2μm (5) Optimize die head heating ring layout to ensure uniform temperature (6) And strengthen process monitoring; on the original basis, additional attention is needed, paying special attention to parameter stability
الخلاصة الأساسية
Die head flow channel design needs to ensure uniform melt distribution and no material stagnation, and the die head should be redesigned when necessary. Targeted preventive measures need to be taken in different production scenarios.
die head flow channeluniform flow velocitysizing sectionflow channel dead cornertemperature uniformity