Unstable discharge/surging in the polyolefin plastomer extrusion process (Variant: Enhanced Measures)
ظاهرة المشكلة
The extruder discharge is sometimes more and sometimes less, the extrudate is uneven in thickness, and periodic surging occurs.
Unstable discharge directly affects the dimensional accuracy and quality consistency of the product.
In particular, additional attention is needed on the original basis; this problem is more prominent and requires focused attention.
تحليل الأسباب
(1)The conveying in the screw feeding section is unstable and the solid bed breaks
(2)The hopper feeding is not smooth and the raw material bridges
(3)The barrel temperature setting is improper, and the feeding section temperature is too high or too low
(4)The screw speed fluctuates
(5)The raw material particle size is uneven or contains too much powder
(6)On the original basis, additional attention is needed: fluctuations in process parameters or changes in equipment status have aggravated this problem
الحل
(1)Optimize the barrel temperature distribution, and appropriately lower the feeding section temperature to prevent premature melting
(2)Install a vibrator on the hopper to prevent bridging and ensure continuous feeding
(3)Reasonably set the temperature of each section of the barrel to ensure it is within the range of 180-230°C
(4)Check the extruder drive system and stabilize the screw speed
(5)Control the uniformity of raw material particles, with the powder proportion not exceeding 5%
(6)And strengthen process monitoring; on the original basis, additional attention is needed to pay special attention to parameter stability
الخلاصة الأساسية
Unstable discharge is caused by unstable solid conveying, and the barrel temperature and feeding system need to be optimized.
Targeted preventive measures need to be taken in different production scenarios.