Cross-linked polyethylene pipe pressure resistance test unqualified
ظاهرة المشكلة
The pipe ruptures or leaks in the hydraulic test, and the pressure resistance performance is not up to standard.
Unqualified pressure resistance directly threatens the safety of pipe use and is a fatal defect in water supply and gas pipelines.
تحليل الأسباب
(1)The pipe wall thickness is insufficient or uneven
(2)Material degradation causes the molecular weight to decrease
(3)There are bubbles or impurities in the pipe
(4)The crystallinity is inappropriate and the mechanical properties are poor
(5)The melt plasticization is insufficient and the welding is poor
الحل
(1)Check and adjust the pipe wall thickness to ensure the wall thickness of each part is uniform and up to standard
(2)Control the extrusion temperature within the range of 170-220°C to avoid material degradation
(3)Fully dry the raw material to ensure the raw material is clean
(4)Optimize the cooling conditions to ensure the crystallinity of the cross-linked polyethylene is appropriate
(5)Optimize the screw design to ensure sufficient plasticization
الخلاصة الأساسية
Unqualified pressure resistance is caused by insufficient wall thickness, material degradation, or internal defects, and needs to be solved systematically from process and material quality.