Injection Molding
13 مشاهدة
Improper barrel temperature setting for PBT '2079851475616104452
ظاهرة المشكلة
Too high barrel temperature causes material degradation, color deepening, and performance decline; too low causes poor plasticization.
تحليل الأسباب
The processing temperature window of PBT is narrow (230-270°C); exceeding the upper limit makes it easy to degrade, and below the lower limit the plasticization is poor.
الحل
Set strictly according to the recommended temperature of 230-260°C; use decreasing temperature control (high at the rear and low at the front); regularly calibrate the temperature control system.
الخلاصة الأساسية
PBT temperature control accuracy directly affects product quality.