ظاهرة المشكلة
Frequent breakage during PET melt spinning, poor production continuity, uneven fiber quality.
تحليل الأسباب
Gel particles or impurities in the melt, improper spinning temperature, filter screen clogging, unstable cooling conditions.
الحل
Improve filtration accuracy (20-40μm filter screens), optimize spinning temperature 280-295°C, control melt residence time <15min, stabilize side-blowing air.
الخلاصة الأساسية
PET spinning breakage is a comprehensive reflection of raw material purity, temperature, and filtration.