Molding Process
7 مشاهدة
Uneven solid-state polycondensation of PET chips
ظاهرة المشكلة
After solid-state polycondensation (SSP) of PET chips, the IV value distribution is wide, and some chips have low IV.
تحليل الأسباب
Temperature distribution in the solid-state polycondensation reactor is uneven; uneven chip particle size causes reaction rate differences; gas flow distribution is uneven.
الحل
Optimize reactor design and temperature control; sieve to control particle size deviation to ±10%; optimize gas flow distribution; precisely control reaction time.
الخلاصة الأساسية
PET solid-state polycondensation uniformity is key to bottle-grade chip quality.