Extrusion & Post
5 مشاهدة
Insufficient peel strength of PET extrusion coating
ظاهرة المشكلة
PET extrusion coating on other substrates (paper, aluminum foil) has insufficient peel strength and easily delaminates.
تحليل الأسباب
PET melt has poor adhesion to the substrate; the substrate surface is untreated or insufficiently treated; coating temperature is on the low side and wetting is insufficient.
الحل
Corona or flame treat the substrate to increase surface energy; increase coating temperature to improve wettability; increase laminating roller pressure.
الخلاصة الأساسية
PET extrusion coating bonding requires dual guarantees of substrate surface treatment and process temperature.
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!