Material Drying 7 مشاهدة

The dry-state PA impact strength is low and conditioning toughening is required

ظاهرة المشكلة
The dry-state PA impact strength is low and conditioning toughening is required
تحليل الأسباب
In the dry state of polyamide 410 (bio-based long carbon chain nylon), the moisture content is low, the plasticizing effect of water molecules is missing, and the impact strength is only 1/3-1/2 of that in the wet state The moisture content of products just after demolding is extremely low, and the brittleness is extremely high The dry-state brittleness is more severe in low-temperature environments Thin-walled products have a higher risk of dry-state brittle fracture Rapid demolding followed by external force causes immediate brittle fracture
الحل
Perform conditioning treatment after demolding to bring the moisture content to 1.5-2.5% Avoid applying force and impact to products just after demolding Special conditioning is required for use in low-temperature environments Extend the conditioning time for thin-walled products Avoid dry-state stress during transportation and storage
الخلاصة الأساسية
PA dry-state brittleness requires conditioning treatment before use
dry-state impactconditioningbrittlenessPA