Material Analysis 5 مشاهدة

Quality fluctuation caused by regrind use of high impact polystyrene

ظاهرة المشكلة
After using regrind, product quality fluctuates, color changes, strength decreases, or black specks appear.
تحليل الأسباب
(1) Regrind repeatedly processed many times, molecular weight gradually decreases (2) Different materials or impurities mixed into the regrind (3) Regrind pelletizing temperature too high, material partially degrades (4) Uneven regrind particle size, unstable feeding (5) Regrind ratio too high or inconsistent
الحل
(1) Control regrind ratio not exceeding 15-20% (2) Regrind used no more than twice repeatedly (3) Regrind stored by classification, different materials must not be mixed (4) Regrind pelletizing temperature controlled at the lower value within the 180-240°C range (5) Regrind sieved after crushing
الخلاصة الأساسية
Regrind use needs to control ratio and number of times; classified management is key.