Processing Machinery 8 مشاهدة

Color difference/unstable color of high impact polystyrene ABS products

ظاهرة المشكلة
ABS product color is unstable, color difference appears between different batches or within the same batch, affecting product appearance consistency.
تحليل الأسباب
(1) Poor dispersion of color masterbatch particles (2) Processing temperature fluctuation causes different pigment dispersion (3) Inconsistent regrind ratio (4) Different raw material base colors (5) Insufficient screw shear
الحل
(1) Use color masterbatch particles with good dispersibility (2) Stabilize processing temperature within the 180-240°C range (3) Unify regrind ratio (4) Use raw material from the same batch (5) Use a mixing-type screw
الخلاصة الأساسية
ABS color difference is caused by uneven pigment dispersion and process fluctuation.
color differenceABScolor masterbatch dispersionprocessing temperaturemixing screw