MBS core-shell structure destroyed during processing

ظاهرة المشكلة
MBS core-shell structure is destroyed during processing, and the toughening effect is completely lost
تحليل الأسباب
Processing temperature too high, exceeding the 180-220°C upper limit, causing rubber core melting Excessive screw shear destroys the core-shell interface Mixing time too long, core-shell structure repeatedly stressed and destroyed Screw compression ratio too large Improper MBS model selection, fragile core-shell structure
الحل
Strictly control processing temperature not exceeding the 180-220°C upper limit Reduce screw rotation speed to reduce shear Shorten mixing time Select a low compression ratio screw Select MBS models with stable core-shell structure
الخلاصة الأساسية
MBS core-shell structure needs gentle processing conditions for protection
core-shell structuretoughening failureshear protectionMBS