Extrusion & Post
6 مشاهدة
PAN spinning solution gelation
ظاهرة المشكلة
PAN solution locally gels during storage or spinning and loses spinnability
تحليل الأسباب
Temperature fluctuations cause PAN crystallization and physical crosslinking; the solvent system (such as DMSO/DMF/NaSCN aqueous solution) has reduced dissolving ability for PAN; PAN concentration too high
الحل
Strictly control the spinning solution temperature at 60-80°C; select suitable solvent concentration and PAN content (usually 15-25%); filter to remove gel particles
الخلاصة الأساسية
Gelation of PAN solution is the main process risk in carbon fiber precursor spinning
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!