Processing Machinery
7 مشاهدة
Product black spots/burnt spots
ظاهرة المشكلة
Black or dark brown spots appear on the product, accompanied by burnt odor, with local material carbonization
تحليل الأسباب
Processing temperature >400°C causes PEEK thermal decomposition and carbonization; material stays in the barrel too long (>5min); heater band temperature control accuracy insufficient, producing hot spots
الحل
Strictly control the maximum barrel temperature ≤400°C; shorten the total material residence time to ≤5 minutes; use a PID precise temperature control system (accuracy ±1°C)
الخلاصة الأساسية
Once PEEK thermal degradation occurs, it is irreversible and causes permanent damage to the product
هل كان هذا مفيدًا؟
0 شخص وجدوا هذا مفيدًا
شكرًا لك على ملاحظاتك!