Material Drying 7 مشاهدة

Insufficient melt flowability, mold filling difficulty

ظاهرة المشكلة
The melt cannot fill thin-wall or complex geometry cavities
تحليل الأسباب
Processing temperature too low (<360°C), the material is not fully melted to a low-viscosity state; PEEK grade molecular weight too high (such as medium-high viscosity injection grades); moisture affects plasticization
الحل
Increase the processing temperature to 370-390°C to improve flowability; select low-viscosity PEEK grades (such as 150G or 90G); fully dry to ensure the material state before plasticization
الخلاصة الأساسية
PEEK's high melting point determines that extremely high processing temperature and pressure are required to ensure flowability
flowabilityprocessing temperaturemelt viscositymolecular weightPEEK grade