Q
Difficult Demolding in PU '2079851475616104452
Q
Periodic EVOH Surface Ripples
A
Ripples are caused by unstable injection; equipment overhaul and PID control are key
Injection Molding EVOHsurface rippleinjection stabilityequipment overhaulPID control
Q
EVOH Surface Tiger Stripes
A
Tiger stripes are caused by unstable injection front; multi-stage injection and high mold temperature are key
Injection Molding EVOHtiger stripeinjection speedmulti-stage injectionmold temperature control
Q
Obvious EVOH Surface Color Difference
A
Color difference is caused by uneven dispersion and orientation; masterbatch method and stable processing are key
Injection Molding EVOHcolor differencecolor masterbatch dispersionpigment orientationtemperature stability
Q
EVOH Surface Orange Peel
A
Orange peel is caused by rapid cooling and solidification; increasing mold temperature and holding pressure are key
Injection Molding EVOHorange peelmold temperatureholding pressuresurface solidification
Q
Severe Internal Stress Concentration in EVOH
Q
Unstable Weight of EVOH Injection Molded Products
A
Product weight stability depends on shot volume precision and holding consistency
Injection Molding EVOH injectionweight fluctuationshot volumeholding consistencyV/P switchover
Q
EVOH '2079851475616104452 Cold Slug Marks
Q
EVOH '2079851475616104452 Flow Marks
Q
EVOH '2079851475616104452 Sink Marks
ChemAI