Q
PAEK insufficient mold filling flow
A
PAEK requires a processing temperature sufficiently above Tm to ensure flowability
Molds & Tooling mold fillingflowmelt temperaturemold temperaturethreshold temperature
Q
PAEK high-temperature degradation producing black spots
A
PAEK thermal degradation is as irreversible as PEEK
Processing Machinery black spotsdegradationtemperature controlresidence time
Q
PAEK insufficient crystallinity, low performance
A
PAEK crystallinity is the most important performance control indicator
Molds & Tooling crystallinityamorphousmold temperaturepost-processing
Q
PAEK product bubbles/internal pores
Q
LGFPP processing comprehensive problem - injection speed
A
Q
LGFPP processing comprehensive problem - mold temperature
Q
LGFPP processing comprehensive problem - screw wear
A
Q
LGFPP processing comprehensive problem - glass fiber orientation
A
The processing quality management of LGFPP materials requires comprehensive attention to multiple dimensions such as glass fiber orientation
Processing Machinery LGFPPglass fiber orientationprocessing qualityprocess optimizationequipment management
Q
Product creep performance substandard
A
The creep performance of LGFPP depends on effective load transfer of the fiber skeleton
Molding Process creepconstant loadstress relaxationhigh molecular weight PPfiber orientation
Q
Long glass fiber poor impregnation causing dispersion difficulty
A
Full impregnation of fibers is the prerequisite for exerting the reinforcement effect
Injection Molding impregnationwetting anglepre-impregnationlow molecular PPscrew design