إجابات عملية على التحديات الشائعة في مواد البلاستيك

11636 سؤال
Q
Improper processing temperature window selection for metallocene linear low-density polyethylene metallocene linear low-density polyethylene (variant: strengthened measures)
Q
Metallocene linear low-density polyethylene MLLDPE high extrusion torque/high energy consumption (variant: mass production scenario)
Q
Metallocene linear low-density polyethylene MLLDPE high extrusion torque/high energy consumption (variant: startup commissioning scenario)
Q
Metallocene linear low-density polyethylene MLLDPE high extrusion torque/high energy consumption (variant: strengthened measures)
Q
Unstable cooling line height of linear low-density polyethylene film
Q
Uneven cutting end face of linear low-density polyethylene pipes
Q
Gel particles/gel appearing in linear low-density polyethylene film
Q
Cooling system efficiency decline of linear low-density polyethylene extruder
Q
Sizing device failure of linear low-density polyethylene extruder
A
Sizing device failure needs to be solved from three aspects: vacuum system, cooling system and mold precision.
Molding Process sizing devicevacuum degreesizing sleeve wearcooling watermold concentricity
Q
Unreasonable head flow channel design of linear low-density polyethylene extruder
A
Head flow channel design needs to ensure uniform melt distribution and no stagnation; redesign the head if necessary.
Production & Quality head flow channeluniform flow velocityland sectionflow channel dead zonetemperature uniformity