HDPE product low-temperature brittle cracking

Problembeschreibung
HDPE products crack when used in winter.
Ursachenanalyse
HDPE has high crystallinity and reduced low-temperature toughness; notch-sensitive, sharp corners easily crack at low temperature.
Lösung
①Select high-impact grades for low-temperature applications; ②eliminate sharp corners in the structure; ③conduct low-temperature drop verification; ④avoid large deformation assembly at low temperature.
Wichtigste Erkenntnis
Low-temperature applications: grade selection + rounded corners as double insurance.
HDPE; low temperature; brittle cracking; impact resistance; sharp corners